anvilfire.com flaming anvil trademark logo copyright (c) 1998 Patrick J. Dempsey
     HOME!  |  STORE  |  Getting Started in Blacksmithing  
 
   Guru's Den   
   V.Hammer-In   
   Slack-Tub Pub II   
   Tailgate Sales   
   FAQs   
   Glossary   
   Links   
   NEWS!   
   Plans   
   Armoury   
   iForge How-To    
   Health and Safety   
   Book Reviews    
   eBooks On-line   
   Anvil Gallery   
   Vice Gallery   
  Calendar of Events  
   Story Page   
   AnvilCAM - II   
  Touchmark Reg.  
   Power Hammers   
   What's New   
Comic of the Week
   Daily Comics   
Daily Metalworking Comics!
   Webring Nexus   
   Our Sponsors   
anvilfire.com General Site
Welcome visitor from
United States Flag
United States
Country Counter

Tell them you found it on anvilfire.com!


Anvils, Amboß Amboss, l'enclume, incudine, el yunque, bigornia,
städ, incus, aambeeld, batente наковальня



Monkey Head Swage or Coconut for repousse'
Anvils in America, THE book about anvils



anvilfire.com Anvil Gallery

anvilfire donated images

Söderfors Paragon Anvil

soderfors paragon with hammer

124 lb. Söderfors Paragon Anvil made in Sweden

Photos from Kenneth

How do you identify a Söderfors

1) The general shape. Very Swedish/American
2) It is cast steel, too hard and has had the typical chipping.
3) It is marked in pounds (for export to the US or England).
4) It has flats on the top of the feet similar to Peter Wright anvils.
5) It is a cast anvil with handling holes.
6) Markings are stamped in (not typical of a casting).

WEIGHT : 124 lbs. (56.25 kg)?
MADE IN: 1929