p.138 HAND - FORGING Fig. 86. Sinking-Tool of 3/4-in. square or hexagonal tool steel. The sink at the .top is filed smooth without any sharp corners and is about || in. wide and half as deep. The tool is to he caught in a vise. A top tool is also used, to fit into the sink in the lower one. This tool is shown in Fig. 87. It is simply a small Fig. 87. Top Tool