Hand Forging by Thomas F. Googerty

TWISTS, SPIRALS, uniform heat, twisted, bars, handles, pokers, shovels, square iron, twisted, swages, flat stock, grilles, oval, form, tapered, square, tools
   About the Book   
   Book Cover   
   Frontispiece   
   Table of Contents   
    < PREV          NEXT >   



    < PREV          NEXT >   

TWISTS AND SPIRALS 81 to a uniform heat and twisted. Twists of this kind, with possibly more bars, make very nice handles for pokers and shovels. At B a piece of 1/2-in. square iron is twisted. At C a piece of Fig. 46- Section of a Twisted Bar and Tools Used in Swaging flat stock has been used. This kind of stock twisted is better for gates and grilles. At D a piece of 5/8-in. oval has been used. This form is very good for handles of shovels, especially if it be swelled or tapered. At E is a very pleasing twist. It is a piece of 1/2-in. square with a bead swaged lengthwise on its four sides. A section of this is shown in Fig. 46, also the tools used to

Page Counter All Page Counter anvilfire.com General Site
Copyright © 2009 anvilfire.com