Working in Metals by Charles C. Sleffel

Chapter XXI, ch.21, First Problems in Forging., How to make a Stake pin., projects, Stake pins are used for holding ropes in place such as those on tents. wrought, iron, hand hammer, sketch, tapering, fire, hearth, reducing
   About the Book   
   Book Cover   
   End Paper Art   
   Table of Contents   
    < PREV          NEXT >   



    < PREV          NEXT >   

Learning metalworking, metalcraft. Metal trade education. Hobbysmith.
THE BLACKSMITHS SHOP: First Problems in Forging. Chapter XXI, ch.21, First Problems in Forging., How to make a Stake pin., projects, Stake pins are used for holding ropes in place such as those on tents. wrought, iron, hand hammer, sketch, tapering, fire, hearth, reducing