ITC 100

ITC-148 ITC-200 ITC-213 ITC-296A

ITC 100 HT Ceramic Coating

Our most versatile high temperature coating has proven to achieve outstanding energy savings and refractory protection. Use it alone and as a base coat for other ITC products. Applications include coating Kaowool, Inswool or other soft friable refractories including lightweight castable and insulating bricks to make a hard reflective surface. It improves the IR reflectivity of Satanite forge linings. Stocked in pint jars and half gallon buckets. Gallons available on order.

Directions

Prepare Surface: Remove all loose and weakened fiber and bricks, debris, particles, dust and grease from interior walls, door, crown, floor and grooves behind electrical elements. Immediately before applying ITC-100, dampen these areas by spraying lightly with water.

Mix: To one pint of ITC-100 add one-half pint of water and mix well.

Apply: Spraying is the best method of application. Sprayguns are available from ITC. For small applications a brush can be used. Dip the brush in water first each time.

Coverage: 50 to 100 sq. ft. per gallon (6 to 12 sq.ft per pint).

[ Application Details ] : Click for more information.

[ ITC-100 MSDS ] : Click for Material Safety Data Sheet.
 
ITC Products
Products of International Technical Ceramics, Inc.