An excellent durable compound  used to repair broken, chipped or cracked brick, castable or fiber material. Bonds rapidly and eliminates need for costly rebricking and lengthy downtime. Revives old equipment economically and efficiently.

Directions

Prepare Surface: Apply ITC 100 as a base coat.

Apply: Immediately after application of ITC 100, using a spatula or similar tool, fill all the cracks, holes, crevices and damaged areas with the ITC 200. Allow to dry.

Coverage: Depends upon extent of repairs.