ITC 213 Ceramic Coating For Metals

An outstanding product especially formulated to protect metals and graphite, including those exposed to molten metals. It helps to prevent stainless steel and steel parts from erosion, oxidation and fatigue from prolonged use. Protects forge burner nozzels, "pipe" crucibles and electric heating elements. Stocked in pints.

Directions

Prepare Surface: Remove all loose rust layers, grease, dirt and molten metal build-up. If possible, roughen surface to be coated by using a file or hacksaw blade. Sandblasting is NOT recommended by ITC. Wash surface with a 1:1 solution of liquid Clorox Bleach and water.

Mix: To one pint of ITC-213 add one-third pint of water and mix well.

Apply: Mix coating thoroughly. The best results are obtained by using a paint edger or a piece of cloth dipped into the ITC-213 and then vigorously rubbing the coating onto the surface as thinly as possible. A spraygun can be used for applications on large surfaces. Heavy application sprayguns are available from ITC. For thin and small area applications such as molds a standard canister type spraygun is used.

Coverage: 150 to 250 sq. ft. per gallon (~18 to 30 sq.ft per pint).