ITC 296A Ceramic Top Coating

A high purity coating which gives a clean firing and minimizes impurities in gloss kilns and molten metal operations. Use to prevent dross and slag build-up and heavy suds and carbon deposits. ITC-100 and 296A improve the IR reflectivity of all forge and furnace linings improving fuel efficiency and overall throughput.

Directions

Prepare Surface: Apply all other ITC products as recommended.

Mix: To one gallon of ITC 296A add one-half gallon of water and mix well.

Apply: Spraying is the best method of application for large areas. Sprayguns are available from ITC. For small surfaces a brush can be used or a standard canister type spray gun.

Coverage: 100 to 200 sq. ft. per gallon (~12 to 24 sq.ft/pint).
 