EMBOSSED WORK p.149 so that one jaw will bear on the leaf and the other on the bar. The blast is turned on slowly, bringing the whole to a red heat. A little flux is then put onto the top part of the leaf and the heat Fig. 96. Border for Marble Table-Top raised. It is welded on the anvil horn with a small hammer. In raising the heat to the welding point care must be taken not to burn the tines of the leaf.