SAFETY - I : A Case study

Demonstration by Jim Paw-Paw Wilson
http://www.paw-paws-forge.com
August 23, 2000 - Updated August 2002
 

Figure 4
OK, Ladies & Gentlemen, let's get started. Contrary to popular opinion, this is what we're going to be working on tonight. It's just a simple camp fire pot lifter, 12" of 1/4" cold rolled square stock. This is what a finished piece looks like.

Figure 5
And this is what an identical piece looks like after a wire wheel wraps it around the blacksmith's head!

Figure 2
Oh! In case you're curious, this is what the head looks like. Front view first.

Figure 3
And side view second.

Figure 6
Now take a look at an expensive pair of safety glasses.
JIM
WILSON
You can't see them very well, but note the crooked place to the left of center. The largest part of the lens is laying between the ear pieces, and the nose pice (one of them) and three other pieces of lense are there also.
Ten Hammers
Soft tissue only Jim ?

Figure 9
Thanks to the safety glasses, this is what they eye looks like up close. WITHOUT the safety glasses, I'd no longer have the eye!

Figure 7
A little further away, just to show how close it was.
JIM
WILSON
folks, I'm not showing these pictures out of some perverted form of vanity, I'm showing them to make an important point.

YOU CAN'T BE TO CAREFUL!
JIM
WILSON
I was doing all the right things. I had on GOOD safety glasses (THANK GOD!) I was wearing leather gloves. I was not standing in line with the wheel when it grabbe, I was standing to the side.
JIM
WILSON
If I had not been doing all of those things, I wouldn't be sitting here typing, I'd be in the hospital getting used to seeing with one eye. If I was lucky!
JIM
WILSON
For those of you who don't know it, let me teach you a code word.

BRAS.

No, not a double barrelled sling shot!

B Bleeding

R Respiration

A Air way

S Shock
JIM
WILSON
After you ascertain that the patient is breathing, control the bleeding! In this case I used a leather gove. Wasn't clean, but I had it on my hand!

Figure 8
JIM
WILSON
Then I consiously controlled my breathing to avoid hyper-ventilating. Air way was OK. Walked to the house, (While screaming "Sherron!")
JIM
WILSON
She came out, I said "Towel for compress" She grabbed two from kitchen, handted them to me, I threw the glove down, applied pressure. Then said "Transport! Aegis" (Urgent care facility less than a block from the house.) Sher's been with me long enough that she asked NO question, just did exactly as told.
JIM
WILSON
I didn't mention a leather apron because I wasn't wearing one. I should have been. I didn't ment6ion a quilted welders cap because I forgot it. I was wearing it. If you want to remain whole, you MUST get and USE the equipment.

Wire wheels and grinders are probably the most dangerous tools in our shops. I use mine every day. It's a 6" braided wire cup brush on a shaft that's pulley run by a 1750 RPM moter. I felt like it's was safe as possible. It isn't! It'll have some deflector added before I turn it on again!
JIM
WILSON
I always warn other's that this wheel will eat you alive. Just how safe is it really, if I have to warn folks about it. How many tools do you have in YOUR shop that you warn other folks about? How safe are they.
JIM
WILSON
Where is your first aid kit? Do you HAVE a first aid kit in your shop? If not, why the heck not?!? How would you get help if you needed it. Where would you go if you got hurt?

THINK ABOUT THESE THINGS! Plan for the worst! It sure can happen!
JIM
WILSON
Full face shield probably wouldn't have helped Jim. Would have shattered, I think.

Steve, 18 in four separate lacerations. Most over the temple at the corner of the Optical Orb.
Ten Hammers
Jim, ABCDE works well too. Airway, Breathing, Circulation (Pulse), Disability ( what kind) and expose ( or in this case direct pressure to control bleeding). Glad you walkin, talkin, seein, and typin !
hotforge101
jim wilson jim you look al;most as good as the guy we had to cut out of his pick up tonight went haqlf way in to the house with the truck drunk as a skunk
Steve C
How many stiches did it take to close it up? looks pretty bad
JIM
WILSON
Opthalmologist checked me this morning. No retinal separation. But would have definitely ruptered the orb and fractures the Maxillary Process without the glasses.

OBTW. I stopped at the Opticians as I was leaving the Dr's Office and ordered an identical pair of safety glasses. I won't work until they arrive. Jim, I've already considered that and I agree with you. Will do that in addition to the deflectors.
JIM
WILSON
Anybody else? Folks, I was lucky! LEARN from my accident. Tom, When you do, would you mind sending it to Jock for posting on the plans page? Jock is that a good idea?

Jim, I hope you heal fast and don't scar too much
JIM
WILSON
When you're tired, QUIT! That last little bit is when you are in the most danger. Shortcut's are rarely shortcuts. They'r usually longcuts! They will cost you more time, effort and pain than they are usually worth!
JIM
WILSON
OK folks, this was short and very basic. I'd suggest a short course in first aid at your local Red Cross. Then walk through your shop with a very critical eye on safety issues. Let me leave you with one final thought.

You can walk with a plastic leg.

You can work with a plastic arm.

You CAN'T see with a plastic eye!


ADDENDUM,

It is now two years since this accident. As it turns out, the night I did the above demo, all of the damage hadnít shown up yet. I did have a small, star shaped fracture of my skull at the initial impact point. I also had not one but two concussions. One at the initial impact point, the second on the top of my head where I hit a five gallon bucket of concrete when I dove away from the hit.

The accident effectively side lined me for almost two years. I suffered almost constant traumatic head aches for nearly 18 months. Itís only in the last six months that theyíve slowed down enough to permit me to start working again.

In 62 years, Iíve had a total of 7 major head injuries, including two skull fractures. As a result, I have two small lesions on the brain. Not bad enough to require surgery, but they could have been. Iím fortunate that I have a pretty hard head, or Iíd probably be dead by now. (Grin)

BE CAREFULL!!!

-GURU
NOTE: Most injuries involving electric shock are the result of the involuntary spasm that sends you flying. Where the voltage is not high enough to kill you instantly or the path of the current does not stop your heart it is the secondary injuries that hurt many. Head injuries such as Jim's are common in these cases. -guru


iForge is an Andrew Hooper Production
HTML Copyright © 2000 Jock Dempsey, www.anvilfire.com
Webmaster email: webmaster@anvilfire.com

Page Counter     Back to iForge

GSC