Black Beauty P75 Forge Burner
Simple Forge Burner
Quantities are listed above in order to ship Flat Rate. Shipping on 1 through 3 burners is $15.

Black Beauty P75 Forge Burner

Temporarily OUT OF STOCK

Designed and manufactured by Jock Dempsey the anvilfire guru.

The Black Beauty P-75 Forge Burner is a plain 3/4" (pipe size) atmospheric pipe burner designed to be as good as any propane forge burner and simplified to be the most economical on the market.

Capacity: 320 to 500 cuin.

Operating Range 3 to 25 PSIG

Connection: 1/4-18 NPT

Dimensions: 1.050 DIA. by 8-3/4" (26.7mm dia x 222mm)

Mounting: User option (weld on bracket, flanges, compression joint). Drawings on-line.

Package Includes: Burner, mounting and operating instructions.

Warranty: Materials and Construction, 1 Year. Not warranted against burn out due to improper mounting, lack of forge lining maintenance or flash back (burning in mixing tube due to improper operating parameters or installation).

We do not provide a flare with our burners. Our burners are not a hand held torch, they go into a stationary device where a flare is not needed (the refractory lining creating the flare/flame holder).

   P75 Instruction PDF   

   P75 Burner Page   
PayPal Acceptance Mark
 
USPS Priority Mail
DEMPSEYS FORGE, 4714 Granite Trail, Boonville, NC 27011 - 336-367-3499
TERMS  |  PRIVACY  |  ABOUT US  |  CONTACT
Copyright © 1998, 2022 anvilfire.com