EMBOSSED WORK, p.141, petal, hammered, forming, iron, Fig. 89, Essentials, Acanthus, Leaf, bulb, drawing
   About the Book   
   Book Cover   
   Frontispiece   
   Table of Contents   
    < PREV          NEXT >   

 


    < PREV          NEXT >   

EMBOSSED WORK p.141 Each petal is hammered; then the center is heated and hammered on the inside, bringing the points up. The work is allowed to cool and then trued by forming it over the end of a round bar of iron Fig. 89. Essentials of an Acanthus Leaf which has previously been rounded at the end to conform with the shape of the bulb. When this is done the points are bent over as shown in the drawing.