156 HAND-FORGING bending a piece of No. 20 soft steel in cylinder shape, letting the edges butt together. It is then brazed with spelter; afterward it is formed elliptical. The bottom is fitted and brazed. To fasten receiver and base together 3/8-in. square stock is used. The base of the candlestick is round, with the stem riveted into it. The socket to hold the Fig. 103. Candlestick with Raised Projections at Corner of Base